Item | unit | Performance indicators |
Bulk density | g/cm3 | 2.6 |
Compressive strength MPa | 110℃×24h 1200℃×3h | 60 90 |
Line change after burning% | 1200℃×3h | -0.2 |
Wear resistance | Cc | 5 |
SiC | % | 60 |
Item | unit | Performance indicators |
Bulk density | g/cm3 | 2.8 |
Compressive strength MPa | 110℃×24h 1200℃×3h | 120 120 |
Line change after burning% | 1200℃×3h | -0.2 |
Wear resistance | cc | 4 |
Al2O3 | % | 85 |
Item | unit | Performance indicators |
Bulk density | g/cm3 | 2.5 |
Compressive strength MPa | 110℃×24h 1400℃×3h | 70 120 |
Line change after burning % | 1400℃×3h | 0.3 |
Wear resistance | Cc | 7 |
Al2O3 | % | 55 |
Item | unit | Performance indicators |
Bulk density | g/cm3 | 2.5 |
Compressive strength MPa | 110℃×24h 1200℃×3h | 60 100 |
Line change after burning % | 1200℃×3h | -0.2 |
Al2O3 | % | 85 |
Item | unit | Performance indicators |
Bulk density | g/cm3 | 2.3 |
Compressive strength MPa | 110℃×24h 1400℃×3h | 50 50 |
Line change after burning % | 800℃ 1200℃×3h | 0 -0.2 |
Al2O3 | % | 50 |