CH / EN

Ladle refractory

Corundum spinel prefabricated brick (steel wall)


 
Bulk density
Compressive strength
Line rate of change
SoftT4.0
Al2O3+ MgO
110℃×24h
≥2.90g/cm3
≥30.0 Mpa
/
≥1600℃
≥93.00%
1550℃×3h
/
≥50.0 Mpa
±1.0%